Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 745 MPa | 108000 psi | |
Kennametal Stellite Stellite® 31 PM cast Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, miscellaneous we.. |
|||
Tensile Strength, Ultimate | 745 MPa @Temperature 760 °C |
108000 psi @Temperature 1400 °F |
|
Haynes 25 alloy, cold worked sheet, 20% cold reduction, aged at 370°C (700°F) for 1 hour Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Tensile Strength, Ultimate | 746 MPa | 108000 psi | |
Haynes Multimet® alloy, GTAW, 3.2 mm sheet Recommended for use in applications involving high stress at temperatures up to 816°C (1500°F), and moderate stresses up to 1093°C (2000°F). Excellent oxidation resistance, good ductilit.. |
|||
Tensile Strength, Ultimate | 745 MPa @Temperature 650 °C |
108000 psi @Temperature 1200 °F |
|
Haynes 25 alloy, cold rolled and 1205°C (2200°F) solution annealed sheet Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Tensile Strength, Ultimate | 745 MPa | 108000 psi | |
Haynes 556® alloy, bar, after 8000 hours at 870°C (1600°F) Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Tensile Strength, Ultimate | 745 MPa @Temperature 425 °C |
108000 psi @Temperature 797 °F |
|
Haynes Hastelloy® B-3® alloy, 6.3 mm plate The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Tensile Strength, Ultimate | 745 MPa | 108000 psi | |
Special Metals INCONEL® 706 Precipitation Hardening Alloy, Forged Disc, Solution Treated Tensile strength (ultimate and yield), reduction of area, and elongation values reported here are typical for Forged Disc, Solution Treated samples. Density and magnetic permeability are typical of .. |
|||
Tensile Strength, Ultimate | 745 MPa | 108000 psi | |
Wieland 1910 Wilaform Gold Nickel and palladium-free white gold alloy with beautiful white color.Applications: casting, laminar decoration, pipes, tubingDental |
|||
Tensile Strength, Ultimate | 745 - 827 MPa | 108000 - 120000 psi | |
Eagle Brass 770 Nickel Silver 18%, Spring 770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi.. |
|||
Tensile Strength, Ultimate | 744 MPa | 108000 psi | |
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 0% Cold Work Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r.. |
|||
Tensile Strength, Ultimate | 745 MPa | 108000 psi | 0% cold reduction |
ATI Allegheny Ludlum AL 2003™ Duplex Stainless Steel Characteristics: superior stress corrosion cracking resistance to Types 316 and 317, yield strength double that of conventional austenitic stainless steel, good corrosion resistance, good chloride s.. |
|||
Tensile Strength, Ultimate | 747 MPa | 108000 psi | Typical |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 440A, Annealed Allegheny Ludlum Type 440A is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainle.. |
|||
Tensile Strength, Ultimate | 745 MPa | 108000 psi | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 20% Cold Rolled (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Tensile Strength, Ultimate | 745 MPa @Thickness 3.20 mm |
108000 psi @Thickness 0.126 in |
|
Haynes Hastelloy® G-35® Nickel Alloy Sheet, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |