Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 73.0 MPa | 10600 psi | ISO 527 |
LATI LATILUB 88/50-30GRT PEEK Based, 30% Graphite and PTFE Self Lubricating Plastic
(Unverified Data**)&l Latilub self-lubricating plastic materials are designed to replace metals in applications such as gears, bushings, cams, slides, etc., for which, besides their intrinsic properties (moldability, low.. |
|||
Tensile Strength, Ultimate | 73.0 - 130 MPa | 10600 - 18900 psi | Average value: 106 MPa Grade Count:4 |
Overview of materials for PCT, 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT, 40% Glass Reinforced". Specific grades with glass content between 35% and 44% are included. Each pr.. |
|||
Tensile Strength, Ultimate | 73.0 MPa | 10600 psi | ISO 527 |
LATI LATAN 13 G/15 15% Glass Fiber Reinforced Polyoxymethylene Copolymer (POM)
(discontinued **) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Tensile Strength, Ultimate | 73.0 MPa | 10600 psi | |
Lucite International Lucite® 47G Acrylic Bead Resin Lucite® 47G is usually processed as a glass separation resin and has major particle size distribution between 80-100 mesh. It is a methyl methacrylate copolymer.General Lucite® Acrylic Bead R.. |
|||
Tensile Strength, Ultimate | 73.0 MPa | 10600 psi | ASTM D638 |
Lucky CF-920 Acrylic May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and coloring capability. |
|||
Tensile Strength, Ultimate | 73.0 MPa | 10600 psi | ASTM D638 |
Lucky EG-920 Acrylic, Extrusion Grade Special extrusion grade with excellent stress cracking resistance, intended mainly for exterior applications. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, hi.. |
|||
Tensile Strength, Ultimate | 73.0 MPa | 10600 psi | ASTM D638 |
Plenco 6015 Phenolic, Briquette, Injection Molded PLENCO 06015 is a glass and mineral filled phenolic molding compound offering improved mechanical strength, dimensional stability and excellent electrical properties. 06015 is available in black.Inf.. |
|||
Tensile Strength, Ultimate | 73.0 MPa @Temperature 704 °C |
10600 psi @Temperature 1300 °F |
|
AK Steel 409 ULTRA FORM® Stainless Steel AK Steel 409 ULTRA FORM Stainless Steel provides an outstanding combination of improved forming and welding characteristics, while providing superior resistance to oxidation, corrosion, ridging and .. |
|||
Tensile Strength, Ultimate | 73.0 MPa | 10600 psi | ASTM D638 |
A. Schulman ComAlloy Hiloy® 123 Polypropylene, Glass Reinforced, Chemically Coupled, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 73.0 MPa | 10600 psi | ASTM D638 |
Asahi Kasei Delpet® 80N Acrylic Molding Compound, High Heat Grade 80N has high heat resistance and strength. Recommended for taillight lenses, reflectors, and other auto parts, and general lighting fixtures. General Delpet® qualities include attractive transpar.. |
|||
Tensile Strength, Ultimate | 73.0 MPa | 10600 psi | ASTM D638-68 |
Budd Hi-Flex® SMC
(discontinued **) Parts requiring high strength and dimensional stability, excellent surface smoothness without sink marks; parts to be painted requiring an automotive-type finish.Data provided by the manufacturer. |