Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 72.4 MPa | 10500 psi | ASTM D638 |
Plaskolite Optix® CA-86 Clear General Purpose Acrylic Resin General purpose acrylic resin, extrusion and injection molding gradeApplications: A general-purpose acrylic resin designed for high heat application. This resin offers the highest heat resistance a.. |
|||
Tensile Strength, Ultimate | 72.4 MPa | 10500 psi | ASTM D638 |
Plaskolite West Optix® CA-86 Clear General Purpose Acrylic Resin General purpose acrylic resin, extrusion and injection molding gradeApplications: A general-purpose acrylic resin designed for high heat application. This resin offers the highest heat resistance a.. |
|||
Tensile Strength, Ultimate | 72.4 MPa | 10500 psi | ASTM D3574E |
Mearthane Durethaneâ„¢ F DF-255A Closed Cell Foam Polyurethane TDI backbone: ester.Summary: Durethane F is chemically blown urethane closed cell foam. Mearthane can custom formulate Durethane F, varying the physical properties (coefficient of friction, abrasio.. |
|||
Tensile Strength, Ultimate | 72.4 MPa | 10500 psi | ASTM D638 |
Techmer ES Plaslube® J-50/10/TF/10 Polycarbonate, 10% GFR, 10% PTFE |
|||
Tensile Strength, Ultimate | 72.4 MPa | 10500 psi | ASTM Data |
Styron CALIBRE™ 200 4 Polycarbonate, General Purpose CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins .. |
|||
Tensile Strength, Ultimate | 72.4 MPa | 10500 psi | ASTM Data |
Styron CALIBRE™ 200 6 Polycarbonate, General Purpose CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins .. |
|||
Tensile Strength, Ultimate | 72.4 MPa | 10500 psi | ASTM D638 |
Styron CALIBREâ„¢ 201-06 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Strength, Ultimate | 72.4 MPa | 10500 psi | ASTM Data |
Styron CALIBRE™ 300 4 Polycarbonate, General Purpose CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren.. |
|||
Tensile Strength, Ultimate | 72.4 MPa | 10500 psi | ASTM Data |
Styron CALIBRE™ 300 6 Polycarbonate, General Purpose CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren.. |
|||
Tensile Strength, Ultimate | 72.4 MPa | 10500 psi | ASTM D638 |
Styron CALIBREâ„¢ 301-06 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Strength, Ultimate | 72.4 MPa | 10500 psi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 4310-6 Polycarbonate EMERGEâ„¢ PC 4310-6 advanced resin is high-performance polycarbonate resin offering high heat resistance and maximum toughness. Applications: Consumer Electronics and Information Technology Equ.. |
|||
Tensile Strength, Ultimate | 72.4 MPa | 10500 psi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 4510-6 Polycarbonate EMERGEâ„¢ PC 4510-6 advanced resin is a general purpose polycarbonate resin offering ignition resistance, heat resistance and excellent toughness. Applications: Consumer Electronics and Informa.. |
|||
Tensile Strength, Ultimate | 72.4 MPa | 10500 psi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 4530-6 Polycarbonate EMERGEâ„¢ PC 4510-15 advanced resin is a general purpose polycarbonate resin offering ultraviolet light stability, ignition resistance, heat resistance and excellent toughness. Applications: Co.. |
|||
Tensile Strength, Ultimate | 72.4 MPa | 10500 psi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ 2060-6 Polycarbonate CALIBREâ„¢ 2060-6 resin is designed for medical applications which use steam or ethylene oxide for sterilization. This material has excellent retention of physical properties and optical clarity.. |
|||
Tensile Strength, Ultimate | 72.4 MPa | 10500 psi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ 2061-6 Polycarbonate CALIBREâ„¢ 2061-6 resin is used in applications involving steam or ethylene oxide for sterilization - though suitability for use in these applications is dependent upon autoclave cycle times and .. |
|||
Tensile Strength, Ultimate | 72.4 MPa | 10500 psi | ASTM D638 |
Styron CALIBREâ„¢ 302-06 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Strength, Ultimate | 72.4 MPa | 10500 psi | ASTM D638 |
Styron CALIBREâ„¢ 303-06 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Strength, Ultimate | 72.4 MPa | 10500 psi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 4330-6 Polycarbonate EMERGEâ„¢ PC 4330-6 advanced resin is a polycarbonate resin offering ultraviolet light stability, high heat resistance and maximum toughness. Applications: Consumer Electronics and Information .. |
|||
Tensile Strength, Ultimate | 72.4 MPa | 10500 psi | ASTM D638 |
Adell ER-14 Homopolymer Polypropylene, 20% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 72.4 MPa | 10500 psi | ASTM D638 |
Adell ER-34 Homopolymer Polypropylene, 20% Glass Reinforced Data provided by Adell Plastics, Inc. |