Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 7.136 MPa | 1035 psi | post cured- 4 hours at 204°C |
Multibase SILASTIC® C7-4565 VAROX Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tensile Strength, Ultimate | 7.136 MPa | 1035 psi | |