Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 590 - 725 MPa | 85600 - 105000 psi | |
Materion Brush 1915™ Heat Treated Temper Rod, 0.050" - 0.375" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe.. |
|||
Tensile Strength, Ultimate | 590 - 725 MPa | 85600 - 105000 psi | |
Materion Brush 1915™ Heat Treated Temper Wire, 0.050" - 0.375" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°CBrush 1915™ is Brush Wellman's new heat-treatable leaded copper alloy. Enginee.. |
|||
Tensile Strength, Ultimate | 510 - 725 MPa | 74000 - 105000 psi | |
Materion Brush 1915™ Heat Treated Temper Wire, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°CBrush 1915™ is Brush Wellman's new heat-treatable leaded copper alloy. Enginee.. |