Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 34.5 - 68.9 MPa | 5000 - 10000 psi | |
Bulk Molding Compounds BMC 300 Mineral Filled, Glass Reinforced Polyester BMC 300 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. Our Granite-X series of molding compounds bel.. |
|||
Tensile Strength, Ultimate | 48.3 - 68.9 MPa | 7000 - 10000 psi | |
Bulk Molding Compounds BMC 5209-12940 Mineral Filled, Glass Reinforced Polyester BMC 5209-12940 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced.. |
|||
Tensile Strength, Ultimate | 55.2 - 68.9 MPa | 8000 - 10000 psi | |
Bulk Molding Compounds BMC 5307 Mineral Filled, Glass Reinforced Polyester BMC 5307 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a medium impact material produced in .. |
|||
Tensile Strength, Ultimate | 55.2 - 68.9 MPa | 8000 - 10000 psi | |
Bulk Molding Compounds BMC 620M Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 620M molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, and stuffer injection molding It is characterized by high impact strength, good mol.. |
|||
Tensile Strength, Ultimate | 40.0 - 68.9 MPa | 5800 - 10000 psi | Average value: 52.3 MPa Grade Count:14 |
Overview of materials for Nylon 11, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Tensile Strength, Ultimate | 0.800 - 68.9 MPa | 116 - 10000 psi | Average value: 26.1 MPa Grade Count:120 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum a.. |
|||
Tensile Strength, Ultimate | 55.2 - 68.9 MPa | 8000 - 10000 psi | ASTM D638 |
Premix Premi-Glas® 1200-28 Polyester SMC
(discontinued **) Premi-Glas® 1200-28 series is a low profile, 28 % glass reinforced polyester Sheet Molding Compound designed for recreational vehicle body panels applications that require excellent flexibility and.. |