Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 480 - 655 MPa
69600 - 95000 psi
MetalTek MTEK WC 9 Cast UNS J42045 Alloy Steel
Information provided by MetalTek
Tensile Strength, Ultimate 480 - 655 MPa
69600 - 95000 psi
MetalTek WC 6 Cast UNS J24054 Alloy Steel
General structural use.Applications: Cylinders, rolls, hollow shafts.Information provided by MetalTek
Tensile Strength, Ultimate 480 - 655 MPa
69600 - 95000 psi
MetalTek WCB UNS J13345 Cast Alloy Steel
General structural use.Applications: Cylinders, rolls, hollow shafts.Information provided by MetalTek
Tensile Strength, Ultimate 480 - 655 MPa
69600 - 95000 psi
MetalTek WCC Cast 105-85 Alloy Steel
General structural use.Applications: Cylinders, rolls, hollow shafts.Information provided by MetalTek
Tensile Strength, Ultimate 552 - 655 MPa
80000 - 95000 psi
Eagle Brass 725 Copper Nickel Tin, Extra Hard
Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina..
Tensile Strength, Ultimate 538 - 655 MPa
78000 - 95000 psi
Eagle Brass 770 Nickel Silver 18%, 1/2 Hard
770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi..
Tensile Strength, Ultimate 586 - 655 MPa
85000 - 95000 psi
Ametek AM 388™ Alloy (UNS C72650) TD04 Hard
Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and..
Tensile Strength, Ultimate 605 - 655 MPa
87700 - 95000 psi
L direction
ArcelorMittal Speed 35-510 Electrical Steel
Properties: The iCARe™ Speed product family comes with guaranted losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencie..