Polymer Property : Tensile Strength, Ultimate = 593 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 517 - 593 MPa
75000 - 86000 psi
Eagle Brass 19010 XP-150 Copper Nickel Silicon, Extra Hard
19010 is an extreme versatile high performance copper nickel silicon alloy. It has an excellent combination of strength, conductivity and formability. Typical uses include terminals, relays, connect..
Tensile Strength, Ultimate 538 - 593 MPa
78000 - 86000 psi
Eagle Brass 230 Red Brass, Spring
CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste..
Tensile Strength, Ultimate 496 - 593 MPa
72000 - 86000 psi
Eagle Brass 519 Phosphor Bronzes 6%, 3/4 Hard
Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C..
Tensile Strength, Ultimate 510 - 593 MPa
74000 - 86000 psi
Eagle Brass 752 Nickel Silver 18%, 3/4 Hard
Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info..