Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 586 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 517 - 586 MPa
75000 - 85000 psi
Materion BrushCAST® 20C High Strength Casting Alloy (As Cast)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Tensile Strength, Ultimate 517 - 586 MPa
75000 - 85000 psi
Materion BrushCAST® 21C High Strength Casting Alloy (As Cast)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Tensile Strength, Ultimate 517 - 586 MPa
75000 - 85000 psi
Materion BrushCAST® 20CT Fine Grain Casting Alloy (As Cast)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Tensile Strength, Ultimate 503 - 586 MPa
73000 - 85000 psi
Eagle Brass 706 Copper Nickel 10%, Extra Hard
706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to..
Tensile Strength, Ultimate 517 - 586 MPa
75000 - 85000 psi
Ametek AM 388™ Alloy (UNS C72650) TD02 1/2 Hard
Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and..
Copyright © lookpolymers.com All Rights Reserved