Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 483 - 517 MPa
70000 - 75000 psi
Materion BrushCAST® 165C High Strength Casting Alloy (As Cast)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Tensile Strength, Ultimate 483 - 517 MPa
70000 - 75000 psi
Materion BrushCAST® 165CT Fine Grain Casting Alloy (As Cast)
Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr..
Tensile Strength, Ultimate 414 - 517 MPa
60000 - 75000 psi
Materion BrushCAST® 3C High Conductivity Casting Alloy (As Cast & Aged)
Pouring Temperature: 1095-1175°CHeat treatment required for max strength (Annealing): 870-900°C/water quenchHeat treatment required for max strength (Hardening): 870-900°C/water quenchDescr..
Tensile Strength, Ultimate 345 - 517 MPa
50000 - 75000 psi
Materion ToughMet® T3 CA
ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e..
Tensile Strength, Ultimate 434 - 517 MPa
63000 - 75000 psi
Eagle Brass 521 Phosphor Bronzes 8% C, 1/4 Hard
Alloy C521 is a high tin alloy of the phosphor bronze family. The additional tin relative to the more commonly used C510 results in higher mechanical properties with a modest reduction in electrical..
Tensile Strength, Ultimate 379 - 517 MPa
55000 - 75000 psi
Eagle Brass 725 Copper Nickel Tin, 1/4 Hard
Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina..
Tensile Strength, Ultimate 434 - 517 MPa
63000 - 75000 psi
Eagle Brass 735 Nickel Silver 18%, 1/2 Hard
735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company
Tensile Strength, Ultimate 393 - 517 MPa
57000 - 75000 psi
Eagle Brass 762 Nickel Silver 12%, Annealed
762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s..
Tensile Strength, Ultimate 462 - 517 MPa
67000 - 75000 psi
Typical
AK Steel 18 Cr-Cb™ Ferritic Stainless steel
AK Steel 18 Cr-Cb™ provides a more effective solution than Type 409 to many automotive exhaust applications, due to its higher oxidation resistance, improved creep resistance and moderate formabili..
Tensile Strength, Ultimate 413 - 517 MPa
59900 - 75000 psi
Ametek AM 388™ Alloy (UNS C72650) TD01 1/4 Hard
Information supplied by Ametek Specialty Metal Products Division.Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and..
Tensile Strength, Ultimate 441 - 517 MPa
64000 - 75000 psi
AK Steel 436L ULTRA FORM® Ferritic Stainless Steel
AK Steel’s 436L ULTRA FORM® is a ferritic grade of stainless steel that outperforms Type 409 in oxidation resistance and corrosion testing. The addition of molybdenum enhances pitting resistance w..
Copyright © lookpolymers.com All Rights Reserved