Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1.20 - 5.50 MPa
174 - 798 psi
Average value: 2.39 MPa Grade Count:14
Overview of materials for Silicone, RTV, Construction Grade
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Construction Grade". Each property range of values reported is minimum and maximum values..