Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 414 - 483 MPa | 60000 - 70000 psi | |
Eagle Brass 19210 XP-10 Copper Iron, Extra Hard 19210 has higher strengths than most copper alloys but thanks to its composition and processing it retains formability and conductivity that other copper alloys lose. Typical uses include cooling f.. |
|||
Tensile Strength, Ultimate | 414 - 483 MPa | 60000 - 70000 psi | |
Eagle Brass 194 HSM® Copper, Hard High Strength Modified Copper Alloy C194 is a first generation high performance alloy used worldwide. C194 combines good electrical conductivity with high tensile strength, good solderability and pl.. |
|||
Tensile Strength, Ultimate | 379 - 483 MPa | 55000 - 70000 psi | |
Eagle Brass 511 Phosphor Bronzes 4%, 1/2 Hard 511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge.. |
|||
Tensile Strength, Ultimate | 455 - 483 MPa | 66000 - 70100 psi | |
AK Steel 439 Ferritic Stainless steel AK Steel 439 has better oxidation and corrosion resistance than Type 409. This alloy also has optimum formability that is reproducible coil after coil and heat after heat. This provides special ad.. |
|||
Tensile Strength, Ultimate | 379 - 483 MPa | 55000 - 70100 psi | |
Ametek High Purity Nickel Strip 899A 1/4 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Ultimate | 379 - 483 MPa | 55000 - 70100 psi | |
Ametek High Purity Nickel Strip 899L 1/4 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Ultimate | 379 - 483 MPa | 55000 - 70100 psi | |
Ametek High Purity Nickel Strip 899M 1/4 Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |