Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 352 - 421 MPa
51000 - 61000 psi
Eagle Brass 230 Red Brass, 1/2 Hard
CDA 230 is known for having an electrical conductivity of 37% IACS, red color, corrosion resistance, excellent formability and moderate strength. Typical uses include costume jewelry, eyelets, faste..
Tensile Strength, Ultimate 310 - 421 MPa
45000 - 61000 psi
Eagle Brass 260 Cartridge Brass, Annealed
Alloy C260 is commonly used for electrical components, electronic parts, and mechanical fasteners. The alloy has good strength but poor stress relaxation characteristics and does not make a particul..
Tensile Strength, Ultimate 338 - 421 MPa
49000 - 61000 psi
Eagle Brass 510 Phosphor Bronzes 5% A, 1/4 Hard
Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info..