Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 379 - 414 MPa
55000 - 60000 psi
Materion BrushCAST® 3C High Conductivity Casting Alloy (As Cast)
Pouring Temperature: 1095-1175°CHeat treatment required for max strength (Annealing): 870-900°C/water quenchHeat treatment required for max strength (Hardening): 870-900°C/water quenchDescr..
Tensile Strength, Ultimate 345 - 414 MPa
50000 - 60000 psi
Meehanite Almanite® W1 Wear and Abrasion Resisting Cast Iron
Type W1 is an austenitic-martensitic white iron characterized by high hardness and relatively good impact strength. Type W1 has a pearlitic matrix.General Meehanite information - Meehanite metal is..
Tensile Strength, Ultimate 345 - 414 MPa
50000 - 60000 psi
Meehanite Almanite® W2 Wear and Abrasion Resisting Cast Iron
Type W2 is an austenitic-martensitic white iron characterized by high hardness and relatively good impact strength. Type W2 has a martensitic matrix.General Meehanite information - Meehanite metal ..
Tensile Strength, Ultimate 324 - 414 MPa
47000 - 60000 psi
Eagle Brass 19210 XP-10 Copper Iron, 1/2 Hard
19210 has higher strengths than most copper alloys but thanks to its composition and processing it retains formability and conductivity that other copper alloys lose. Typical uses include cooling f..
Tensile Strength, Ultimate 331 - 414 MPa
48000 - 60000 psi
Eagle Brass 519 Phosphor Bronzes 6%, Annealed
Alloy C519 has 6% nominal tin producing higher mechanical strengths with a slight decrease in electrical conductivity when compared to C510 phosphor bronze. Often functionally interchangeable with C..