Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 25.0 - 400 MPa @Strain 1.00 - 10.0 % |
3630 - 58000 psi @Strain 1.00 - 10.0 % |
Average value: 101 MPa Grade Count:5 |
Overview of materials for Nylon 66, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |
|||
Tensile Strength, Ultimate | 25.0 - 400 MPa @Temperature -40.0 - 200 °C |
3630 - 58000 psi @Temperature -40.0 - 392 °F |
Average value: 101 MPa Grade Count:5 |
Overview of materials for Nylon 66, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |
|||
Tensile Strength, Ultimate | 300 - 400 MPa | 43500 - 58000 psi | |
MMCC Al/B4C Particulate Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
Tensile Strength, Ultimate | 330 - 400 MPa | 47900 - 58000 psi | |
SSAB Tunnplat Docol® 220 YP High-strength Steel High-strength SteelComments: Docol YP - Cold Rolled Steel - HSLA. Property values are for cold-rolled steel; thicknesses 0.5 - 3.00 mm. Iron content is approximate - exact composition is not report.. |
|||
Tensile Strength, Ultimate | 345 - 400 MPa | 50000 - 58000 psi | |
Eagle Brass 110 EPT COPPER, Spring Alloy 110, also known as electrolytic tough pitch (ETP) copper, is commonly used in electric current carrying applications. 110 Copper is 99.9% pure copper with an electrical conductivity rating of .. |
|||
Tensile Strength, Ultimate | 331 - 400 MPa | 48000 - 58000 psi | |
Eagle Brass 240 Low Brass, 1/4 Hard CDA 240 has excellent ductility, corrosion resistance and strength which allows it to be deep drawn, etched, stamped, blanked and bent. Typical uses include musical instruments, battery caps, flexib.. |
|||
Tensile Strength, Ultimate | 317 - 400 MPa | 46000 - 58000 psi | |
Eagle Brass 511 Phosphor Bronzes 4%, 1/4 Hard 511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge.. |
|||
Tensile Strength, Ultimate | 320 - 400 MPa | 46400 - 58000 psi | |
CLAL-MSX CUPROROR® TL1 1/4 hard, Copper Alloy Alloy especially suited to applications in electronics and electro technology. This doped copper, displays high electrical and thermal conductivity, good mechanical properties and excellent temperat.. |
|||
Tensile Strength, Ultimate | 345 - 400 MPa | 50000 - 58000 psi | |
Eagle Brass 101 OFE COPPER (Certified), Spring Alloy 101 is known as Oxygen-Free Electronic (OFE). It reaches a minimum of 101% IACS conductivity rating. It is the most expensive out of the 101- 110 group because of its higher purity.Information.. |
|||
Tensile Strength, Ultimate | 345 - 400 MPa | 50000 - 58000 psi | |
Eagle Brass 102 OF COPPER (Non-Certified), Spring Alloy 102 is an oxygen-free copper which has better forming, resistance to hydrogen embrittlement, and brazing characteristics than C110 ETP. C102 has good solder-ability and corrosion resistance an.. |
|||
Tensile Strength, Ultimate | 320 - 400 MPa | 46400 - 58000 psi | |
CLAL-MSX SICLANIC S® TD3 Quenched Copper Alloy, 1/2 Hard SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Tensile Strength, Ultimate | 345 - 400 MPa | 50000 - 58000 psi | |
Ametek High Purity Nickel Strip 899L Annealed Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Ultimate | 345 - 400 MPa | 50000 - 58000 psi | |
Ametek High Purity Nickel Strip 899M Annealed Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Ultimate | 270 - 400 MPa | 39200 - 58000 psi | |
ArcelorMittal 01 High formability steel for drawing, Cold rolled Available in the following: uncoated (DC01) and electroglavanized (DC01+ZE) Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These product.. |
|||
Tensile Strength, Ultimate | 300 - 400 MPa | 43500 - 58000 psi | |
ArcelorMittal 13 High formability steel for drawing, Hot rolled Available in the following: uncoated (DD13) Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used extensively in the au.. |
|||
Tensile Strength, Ultimate | 340 - 400 MPa | 49300 - 58000 psi | |
ArcelorMittal 195 BH Bake hardening steel, Cold rolled Description: The composition and processing of these steels are designed to promote a significant increase in yield strength during low-temperature heat treatment, particularly paint curing. Arcelor.. |
|||
Tensile Strength, Ultimate | 340 - 400 MPa | 49300 - 58000 psi | |
ArcelorMittal 220 BH Bake hardening steel, Cold rolled Available in the following: uncoated (HC220B), electroglavanized (HC220B+ZE) and Extragal®/Galvannealed (HC220BD+Z)Description: The composition and processing of these steels are designed to promot.. |
|||
Tensile Strength, Ultimate | 270 - 400 MPa | 39200 - 58000 psi | |
ArcelorMittal 51 High formability steel for drawing, Cold rolled Available in the following: Extragal®/Galvannealed (DX51D +Z/+ZF)Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used.. |
|||
Tensile Strength, Ultimate | 340 - 400 MPa | 49300 - 58000 psi | |
ArcelorMittal IF 180 High strength IF steel, Cold rolled Available in the following: uncoated (HC180Y), electroglavanized (HC180Y+ZE) and Extragal®/Galvannealed (HX180YD+Z/+ZF)Description: These steels were designed to provide an excellent combination of.. |
|||
Tensile Strength, Ultimate | 340 - 400 MPa | 49300 - 58000 psi | |
ArcelorMittal IF 220 High strength IF steel, Cold rolled Available in the following: uncoated (HC220Y), electroglavanized (HC220Y+ZE) and Extragal®/Galvannealed (HX220YD+Z/+ZF)Description: These steels were designed to provide an excellent combination of.. |
|||
Tensile Strength, Ultimate | 345 - 400 MPa | 50000 - 58000 psi | |
Ametek High Purity Nickel Strip 899A Annealed Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Ultimate | 340 - 400 MPa | 49300 - 58000 psi | |
ArcelorMittal H 220 Solid solution steel, Cold rolled Available in the following: uncoated (HC220P) and electrogalvanized (HC220P+ZE) Description: Solid solution steels are designed to provide high strength while maintaining good drawability. These ste.. |
|||
Tensile Strength, Ultimate | 49.6 - 400 MPa | 7200 - 58000 psi | Average value: 132 MPa Grade Count:34 |
Overview of materials for Polypropylene, Long Glass Fiber 50% This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include.. |