Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 310 - 379 MPa @Temperature 20.0 °C |
45000 - 55000 psi @Temperature 68.0 °F |
|
H.C. Starck Ultra 76 Alloy (Ta 2.5%W) Benefits: Significantly improved corrosion resistance in HCl and H2SO4 acids.Minimized hydrogen embrittlement rates compared to standard NRC®76Up to 100 times lower in HCl acidUp to 10 times low.. |
|||
Tensile Strength, Ultimate | 276 - 379 MPa | 40000 - 55000 psi | |
Eagle Brass 19210 XP-10 Copper Iron, 1/4 Hard 19210 has higher strengths than most copper alloys but thanks to its composition and processing it retains formability and conductivity that other copper alloys lose. Typical uses include cooling f.. |