Tensile Strength, Ultimate 296 - 352 MPa
43000 - 51000 psi
Eagle Brass 151 ZHC® COPPER, 1/2 Hard
Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c..