Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 77.0 - 281.306 MPa @Temperature -40.0 - 150 °C |
11200 - 40800.1 psi @Temperature -40.0 - 302 °F |
Average value: 104 MPa Grade Count:4 |
Overview of materials for Nylon 6, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E.. |