Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1.50 - 27.0 MPa | 218 - 3920 psi | Average value: 7.37 MPa Grade Count:36 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade". Each property range of values reported .. |
|||
Tensile Strength, Ultimate | 24.0 - 27.0 MPa | 3480 - 3920 psi | |
Biomer P226 PHB Biodegradable Polymer PHB is a isotactic, absolutely linear, thermoplastic homopolyester built of 3-hydroxy butyric acid. The formula of the subunit is -[O-CH(CH3)-CH2-CO]-. PHB is free from even traces of catalysts. P.. |