Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 45.0 - 269.585 MPa @Temperature -40.0 - 150 °C |
6530 - 39100.1 psi @Temperature -40.0 - 302 °F |
Average value: 101 MPa Grade Count:9 |
Overview of materials for Nylon 66, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |