Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 75.0 - 193 MPa | 10900 - 28000 psi | Average value: 93.5 MPa Grade Count:13 |
Overview of materials for Polyetheretherketone, PEEK, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PEEK, Aramid Fiber Filled". Each property range of values reported is minimum and .. |
|||
Tensile Strength, Ultimate | 89.6 - 193 MPa | 13000 - 28000 psi | Average value: 121 MPa Grade Count:58 |