Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 20.0 - 190 MPa @Temperature -40.0 - 250 °C |
2900 - 27600 psi @Temperature -40.0 - 482 °F |
Average value: 85.1 MPa Grade Count:3 |
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an.. |
|||
Tensile Strength, Ultimate | 20.0 - 190 MPa @Thickness 1.00 - 4.00 mm |
2900 - 27600 psi @Thickness 0.0394 - 0.157 in |
Average value: 85.1 MPa Grade Count:3 |
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an.. |
|||
Tensile Strength, Ultimate | 40.0 - 190 MPa | 5800 - 27600 psi | Average value: 113 MPa Grade Count:90 |
Overview of materials for Nylon 6, Glass Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu.. |