Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 105 - 170 MPa

@Temperature 60.0 - 150 °C
15200 - 24700 psi

@Temperature 140 - 302 °F
Average value: 135 MPa Grade Count:1
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value..
Tensile Strength, Ultimate 30.0 - 170 MPa

@Strain 1.00 - 2.00 %
4350 - 24700 psi

@Strain 1.00 - 2.00 %
Average value: 104 MPa Grade Count:1
Overview of materials for Nylon 6, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E..
Tensile Strength, Ultimate 30.0 - 170 MPa

@Temperature -20.0 - 150 °C
4350 - 24700 psi

@Temperature -4.00 - 302 °F
Average value: 104 MPa Grade Count:1
Overview of materials for Nylon 6, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E..
Tensile Strength, Ultimate 35.9 - 170 MPa
5200 - 24700 psi
Average value: 62.9 MPa Grade Count:84
Overview of materials for Nylon 66, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri..
Tensile Strength, Ultimate 105 - 170 MPa

@Temperature 60.0 - 150 °C
15200 - 24700 psi

@Temperature 140 - 302 °F
Average value: 136 MPa Grade Count:1
Overview of materials for Nylon 66, 40% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Carbon Fiber Filled". Specific grades with carbon fiber content between 35% and 44% are in..
Tensile Strength, Ultimate 50.0 - 170 MPa

@Temperature -40.0 - 120 °C
7250 - 24700 psi

@Temperature -40.0 - 248 °F
Average value: 83.0 MPa Grade Count:2
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re..
Tensile Strength, Ultimate 67.6 - 170 MPa
9800 - 24700 psi
Average value: 141 MPa Grade Count:54
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% ..
Tensile Strength, Ultimate 20.0 - 170 MPa

@Temperature -40.0 - 121 °C
2900 - 24700 psi

@Temperature -40.0 - 250 °F
Average value: 70.7 MPa Grade Count:7
Overview of materials for Nylon 6, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..