Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1590 - 1600 MPa | 230000 - 232000 psi | |
Latrobe Lescalloy® HP 9-4-30 VAC-ARC ; 5.75 in RCS Billet Size High Strength Alloy Steel LESCALLOY HP 9-4-30 VAC-ARC steel is a low alloy, high strength steel with a high nickel and cobalt content to promote toughness. The alloy has been designed to have high hardenability, good weldabi.. |
|||
Tensile Strength, Ultimate | 1400 - 1600 MPa | 203000 - 232000 psi | |
SSAB Tunnplat Docol® 1400 DP High-strength Steel The steels are annealed at temperatures between 750°C and 850°C, depending on the grade of steel, and then are hardened by quenching in water. Tempering is the next stage, in which the steel .. |