Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1340 - 1590 MPa | 194000 - 231000 psi | |
Materion Beryllium Copper Alloy 25 Wire; HT (TH04) Temper; 1.3-2.0 mm Diameter (UNS C17200) Treatment required for max strength: 1 hr @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed it.. |
|||
Tensile Strength, Ultimate | 1340 - 1590 MPa | 194000 - 231000 psi | |
Materion Beryllium Copper Alloy M25 Wire; HT (TH04) Temper; 1.3-2.0 mm Diameter (UNS C17300) Treatment required for max strength: 1 hr @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed it.. |
|||
Tensile Strength, Ultimate | 1580 - 1590 MPa | 229000 - 230000 psi | |
Latrobe Lescalloy® HP 9-4-30 VAC-ARC ; 13.5 in RCS Billet Size High Strength Alloy Steel LESCALLOY HP 9-4-30 VAC-ARC steel is a low alloy, high strength steel with a high nickel and cobalt content to promote toughness. The alloy has been designed to have high hardenability, good weldabi.. |
|||
Tensile Strength, Ultimate | 1310 - 1590 MPa | 190000 - 231000 psi | |
Materion Beryllium Copper Alloy M25 Wire; 3/4HT (TH03) Temper; 1.3-2.0 mm Diameter (UNS C17300) Treatment required for max strength: 1 hr @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed it.. |
|||
Tensile Strength, Ultimate | 1240 - 1590 MPa | 180000 - 230000 psi | |
Special Metals DURANICKEL® 301 (UNS N03301) Spring Strip, Aged Tensile strength (ultimate), hardness, and elongation values reported here are typical for Spring Strip, Aged specifically. Other property values are typical of aged DURANICKEL® alloy 301 or the .. |
|||
Tensile Strength, Ultimate | 1310 - 1590 MPa | 190000 - 231000 psi | |
Materion Beryllium Copper Alloy 25 Wire; 3/4HT (TH03) Temper; 1.3-2.0 mm Diameter (UNS C17200) Treatment required for max strength: 1 hr @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its .. |