Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 82.7 - 146 MPa | 12000 - 21200 psi | Average value: 114 MPa Grade Count:4 |
Overview of materials for Nylon 11 with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are includ.. |