Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 10.3 - 14.5 MPa | 1490 - 2100 psi | ASTM D638 |
Multibase Multi-Flex® TPE D 4107 This product is UV stabilized for automotive applications, like fender guards and airbags. The Xenon Arc is 2.5 Delta E, ASTM SAE J1960 1240 KJ/m². Passes Impact resistance test ASTM GM 9032 P at.. |
|||
Tensile Strength, Ultimate | 10.3 - 14.5 MPa | 1490 - 2100 psi | ASTM D638-95 |
Multibase Multi-Flex® TPO 1047-4107 Passed impact resistance 3.4J at -30°C; ASTM GM 9032 P. This product is UV stabilized for automotive applications, like fender guards and airbags.Data provided by Multibase. |