Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 1000 - 1070 MPa | 145000 - 155000 psi | |
Materion BrushCAST® 165CT Fine Grain Casting Alloy (Solution Annealed & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Ultimate | 890 - 1070 MPa | 129000 - 155000 psi | |
Materion Beryllium Copper Alloy 25 Wire; 3/4H (TD03) Temper; 1.3-2.0 mm Diameter (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 890 - 1070 MPa | 129000 - 155000 psi | |
Materion Beryllium Copper Alloy M25 Wire; 3/4H (TD03) Temper; 1.3-2.0 mm Diameter (UNS C17300) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
Tensile Strength, Ultimate | 1000 - 1070 MPa | 145000 - 155000 psi | |
Materion BrushCAST® 165C High Strength Casting Alloy (Solution Annealed & Aged) Pouring Temperature: 1010-1120°CHeat treatment required for max strength (Annealing): 760-790°C/water quenchHeat treatment required for max strength (Hardening): 760-790°C/water quenchDescr.. |
|||
Tensile Strength, Ultimate | 896 - 1070 MPa | 130000 - 155000 psi | |
Special Metals DURANICKEL® 301 (UNS N03301) Half-Hard Strip Tensile strength (ultimate), hardness, and elongation values reported here are typical for Half-Hard Strip specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the.. |