Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 96.5 MPa | 14000 psi | ASTM D638 |
Nylene® Norpex® AX20GF , 20% Glass Reinforced Polyphenylene Ether Description: Norpex® AX20GF us a 20% glass fiber reinforced Polyphenylene Ether. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric.. |
|||
Tensile Strength, Ultimate | 96.5 MPa | 14000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® PS-15GF/000 FR Polybutylene Terephthalate (PBT), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedIgnition ResistantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 96.5 MPa | 14000 psi | ASTM Data |
Dow Questra® EA503 High Heat Syndiotactic Polystyrene, 30% Glass Filled
(discontinued **) QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve.. |
|||
Tensile Strength, Ultimate | 96.5 MPa | 14000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ SF-10CF/15T Polyphenylene Sulfide (PPS), Carbon Fiber Reinforced, PTFE Lubricated
(discon Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 96.5 - 231 MPa | 14000 - 33500 psi | Average value: 170 MPa Grade Count:30 |
Overview of materials for Nylon 612, Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Carbon Fiber Filler". Each property range of values reported is minimum and maximum values of.. |
|||
Tensile Strength, Ultimate | 96.5 MPa | 14000 psi | oriented film |
Honeywell Aegis™ OX High Barrier Nylon
(discontinued **) Description: Aegis OX is an oxygen-scavenging nylon. Oxygen barrier is comparable to a glass bottle with metal crown closure. In addition Aegis OX provides CO2 barrier and possesses glass-like cla.. |
|||
Tensile Strength, Ultimate | 96.5 MPa | 14000 psi | ASTM D638 |
Techmer ES Electrafil® J-50/CF/10/TF/13/SI/2 Polycarbonate, 10% Carbon Fiber Reinforced, 13% PTFE, 2% Silicone |
|||
Tensile Strength, Ultimate | 96.5 MPa | 14000 psi | ASTM D638 |
Techmer ES Electrafil® J-50/CF/10/TF/15 Polycarbonate, 10% Carbon Fiber Reinforced, 15% PTFE |
|||
Tensile Strength, Ultimate | 96.5 MPa | 14000 psi | ASTM D638 |
Adell AT-13 Nylon 66, 15% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 96.5 MPa | 14000 psi | ASTM D638 |
Adell ER-18 Homopolymer Polypropylene, 40% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 96.5 MPa | 14000 psi | ASTM D638 |
Applied Composites 8050 Polyester SMC Industry Application: ElectricalProduct Application: Business MachinesDistinct Features: Radiant Panel, UL 94-VO, Low Shrink, PigmentableInformation provided by Applied Composites Corporation. |
|||
Tensile Strength, Ultimate | 96.5 - 117 MPa | 14000 - 17000 psi | |
Bulk Molding Compounds BMC 680 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 680 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression and stuffer injection molding It is characterized by good moldability, very high impa.. |
|||
Tensile Strength, Ultimate | 96.5 MPa | 14000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ MP-20GF/05T Modified Polyphenylene Oxide (mPPO), Glass Filled, PTFE Lubricated
(discontin Description/Features:Glass Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 96.5 MPa | 14000 psi | ASTM D638 |
Adell AT-33 Nylon 66, 15% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Tensile Strength, Ultimate | 96.5 MPa | 14000 psi | ASTM D638 |
Adell ER-38 Homopolymer Polypropylene, 40% Glass Reinforced Data provided by Adell Plastics, Inc. |