Tensile Strength, Ultimate
9.79
MPa
1420
psi
Dow Corning SILASTIC® 9280/30 KIT PARTS A&B
40 Durometer, 2-part, 1 to 1 mix, translucent Liquid Silicone Rubber.Information provided by Dow Corning