Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 848 MPa | 123000 psi | |
Hogen HM3750 Tungsten-Based Metal Mil Spec T-21014D Class 4; ASTM B-777-99 Class 4; AMS T-21014 Class 4. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal conductivity and a low CTE.. |
|||
Tensile Strength, Ultimate | 848 MPa | 123000 psi | |
Mi-Tech Metals HD18.5 Tungsten-Based Metal Mil Spec T-21014D Class 4; ASTM B-777-99 Class 4; ASTM B-777-07 Class 4; AMS T-21014 Class 4. Slightly Magnetic.Manufactured by powder metallurgy methods. The tungsten base offers high thermal con.. |
|||
Tensile Strength, Ultimate | 848 MPa | 123000 psi | 5.25 in. Test Specimen |
Latrobe Lescalloy® 410Cb High Strength Stainless Steel LESCALLOY 17-4 VAC-ARC steel is a precipitation hardening martensitic stainless steel. A wide range of mechanical properties is available via simple aging within a 900-1150°F (482-621°C) tempe.. |
|||
Tensile Strength, Ultimate | 848 MPa | 123000 psi | |
Haynes Ultimet® alloy, all-weld metal, GMAW weld (spray) Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Tensile Strength, Ultimate | 848 MPa | 123000 psi | |
Special Metals INCONEL® 686 Nickel Superalloy (UNS N06686) Sheet 0.062 in (1.6 mm) Tensile strength (ultimate and yield) and elongation values reported here are typical for 0.062 inch sheet. Other property values are typical of INCONEL® alloy 686.Data provided by the manufactu.. |
|||
Tensile Strength, Ultimate | 848 MPa | 123000 psi | |
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1150M (Heated 760°C/2hr/AC then 621°C/4hr/AC) Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio.. |
|||
Tensile Strength, Ultimate | 848 MPa | 123000 psi | Annealed 1052°C |
Latrobe MP159® Alloy MP159 is an alloy of the Multiphase family of alloys possessing the unique combination of ultra-high strength, ductility and corrosion resistance. Through work strengthening and aging, MP159 alloy .. |
|||
Tensile Strength, Ultimate | 848 MPa | 123000 psi | |
HP Alloys Alloy X, 5% Cold Worked 5% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, and Haynes International. |