Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 84.0 MPa @Temperature 22.0 °C |
12200 psi @Temperature 71.6 °F |
25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® SMC 1500 Unsaturated Polyester UP SMC 1500 is a special SMC for applications calling for high continuous service temperature. The glass level has been selected to combine good mouldability with good strength and stiffness properties.. |
|||
Tensile Strength, Ultimate | 84.0 MPa | 12200 psi | ASTM D638 |
Toyobo Vylopet® EMC415 PET/PBT Blend Key Feature: HB UL-94 ClassApplications: accessory componentsPET/PBT blends suggested for glossy surfaces. General features of Vylopet® include heat resistance, good mechanical properties, high di.. |
|||
Tensile Strength, Ultimate | 84.0 MPa | 12200 psi | |
Covestro Baygal® 90 IK 51 Polyurethane Uses: Suitable for the solid insulation of measuring transducers.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its ne.. |
|||
Tensile Strength, Ultimate | 84.0 MPa @Temperature 180 °C |
12200 psi @Temperature 356 °F |
ISO 527-1/-2 |
DSM Stanyl® TW271B3 (PA46+PTFE)-CF15 15% Carbon Reinforced, Heat Stabilized, Wear and Friction Modified |
|||
Tensile Strength, Ultimate | 84.0 MPa | 12200 psi | ASTM D638 |
A. Schulman ComAlloy Hiloy® 242 SAN, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 84.0 MPa | 12200 psi | ASTM D638 |
A. Schulman ComAlloy Hiloy® 412 Polyester - PBT, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.15% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 84.0 MPa | 12200 psi | ATSM D638 |
Ashley Polymers Ashlene® 830LN Nylon 6 Basic Nylon 6, medium viscosity, lubricated and nucleated for injection molding.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 84.0 MPa | 12200 psi | ASTM D638 |
A. Schulman ComAlloy Comtuf® 611 Nylon 6, Glass Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.13% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |