Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 834 MPa @Temperature 600 °C |
121000 psi @Temperature 1110 °F |
|
Kennametal Stellite Nucalloy® 488V High-Silicon Nickel-Base Hardfacing Alloy Applications include diesel engine valves, and injection mold screws.Nucalloy® alloys are unique, patented, high-silicon, nickel-base hardfacing alloys that are designed to have optimum combinati.. |
|||
Tensile Strength, Ultimate | 834 MPa @Thickness 3.20 mm |
121000 psi @Thickness 0.126 in |
Sheet |
Haynes 282® Nickel Alloy Sheet, Plate and Bar, Solution Annealed Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
Tensile Strength, Ultimate | >= 834 MPa | >= 121000 psi | |
Crucible Steel JIS SUH600 Martensitic Steel Information provided by Crucible Specialty Metals. |
|||
Tensile Strength, Ultimate | 834 MPa @Temperature 427 °C |
121000 psi @Temperature 801 °F |
|
Carpenter Custom 450® Stainless Steel, Condition H1050 (Age Hardened 566°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |