Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 83.4 MPa | 12100 psi | ISO 527 |
Polikim KESTAMID® PA6G Polyamide 6 Kestamid® is also known as Cast Polyamide or Cast Nylon. Kestamid® is an engineering plastic used commonly in all industrial branches for its superior mechanical, physical, chemical and electrical.. |
|||
Tensile Strength, Ultimate | 83.4 MPa | 12100 psi | DIN 53455; ASTM D638 |
Kolon SPESIN® KP213G15HI Multi Reinforced PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Tensile Strength, Ultimate | 83.4 MPa | 12100 psi | DIN 53455; ASTM D638 |
Kolon KOPA® KN1322VO Flame Retardant Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Tensile Strength, Ultimate | 83.4 MPa | 12100 psi | DIN 53455; ASTM D638 |
Kolon KOPA® KN3311 General Purpose Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Tensile Strength, Ultimate | 83.4 MPa | 12100 psi | DIN 53455; ASTM D638 |
Kolon KOPA® KN3311N General Purpose Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Tensile Strength, Ultimate | 83.4 MPa | 12100 psi | ASTM D638 |
SK Chemicals SKYTHANE® U1731C Magnetic Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tensile Strength, Ultimate | 83.4 MPa @Temperature 871 °C |
12100 psi @Temperature 1600 °F |
Longitudinal |
AK Steel NITRONIC® 19-D Duplex Stainless Steel AK Steel NITRONIC® 19D is a stainless steel with a mixed ferrite and austenite structure. This alloy provides high yield strength (65 ksi minimum {448 MPa}),
good drawing and welding characteristi.. |