Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 816 MPa | 118000 psi | Bar |
Haynes 282® Nickel Alloy Sheet, Plate and Bar, Solution Annealed Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |