Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 790 - 940 MPa | 115000 - 136000 psi | Guaranteed, 1/4 t |
Industeel SUPERELSO® 690CR Quenched and Tempered High Strength Steel for Leg Components of Jack-up Rigs Superelso® 690 CR (SE 690 CR) is a 690MPa (100ksi) yield strength quenched and tempered steel adapted for jack-up rig legs of offshore drilling platforms. Superelso® 690 CR is manufactured via.. |
|||
Tensile Strength, Ultimate | 790 MPa @Temperature 650 °C |
115000 psi @Temperature 1200 °F |
|
Haynes 214® alloy, hot rolled solution annealed plate 12.7 mm (1/2 in.) thick Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Tensile Strength, Ultimate | 790 - 930 MPa | 115000 - 135000 psi | |
Materion Brush 60™ 3/4 HT Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation afte.. |
|||
Tensile Strength, Ultimate | >= 790 MPa | >= 115000 psi | |
MetalTek IN® 100 UNS N13100 Centri-Vac Nickel Based Alloy Information provided by MetalTek |
|||
Tensile Strength, Ultimate | 790 MPa | 115000 psi | |
Haynes 556® alloy, 0% cold reduction, 1010°C anneal for 5 minutes Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Tensile Strength, Ultimate | 790 MPa | 115000 psi | Annealed |
Special Metals INCONEL® Alloy C-276 A nickel-molybdenum-chromium alloy with an addition of tungsten having excellent corrosion resistance in a wide range of severe environments. The high molybdenum content makes the alloy especially .. |
|||
Tensile Strength, Ultimate | >= 790 MPa | >= 115000 psi | |
SSAB Tunnplat Domex® 740XP Extra High-strength Cold-forming Steel Extra High-strength Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. Gene.. |
|||
Tensile Strength, Ultimate | 790 MPa | 115000 psi | Typical |
ATI Allegheny Ludlum AL 601™ Nickel-Base Alloy, Annealed at 982°C (1800°F), UNS N06601 Allegheny Ludlum's AL 601 alloy is an austenitic nickel-chromium-iron alloy designed for both heat and corrosion resistance. As compared to AL 600 alloy, the AL 601 alloy has, in addition to increa.. |