Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 752 MPa @Temperature 538 °C |
109000 psi @Temperature 1000 °F |
|
Haynes Ultimet® alloy, 19.1 mm thick plate, SMAW weld Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Tensile Strength, Ultimate | 752 MPa | 109000 psi | |
Haynes Hastelloy® C-22® alloy, transverse, GMAW spray weldment, 23.4 mm thick plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Tensile Strength, Ultimate | 752 - 841 MPa | 109000 - 122000 psi | |
Eagle Brass 762 Nickel Silver 12%, Spring 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Tensile Strength, Ultimate | 752 MPa @Temperature -73.0 °C |
109000 psi @Temperature -99.4 °F |
Longitudinal |
Carpenter 20Cb-3® Stainless Steel Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re.. |