Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 701 MPa | 102000 psi | |
Haynes HR-160® alloy, plate, aged 1000 hours at 871°C (1600°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |