Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 7.20 MPa | 1040 psi | TPE-0153 (ASTM D 412) |
Advanced Elastomer Systems Santoprene® 251-80 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b.. |
|||
Tensile Strength, Ultimate | 7.20 MPa | 1040 psi | ASTM D412 |
Dow Engage® ENR 8556.00 Ethylene-Octene Copolymer Description: ENR 8556.00 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent performance in extrusion applications such as tubing and profiles. This elastomer provides excellen.. |
|||
Tensile Strength, Ultimate | 7.20 MPa | 1040 psi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4640 Low Cost General Purpose Hose FormulationNordel® IP 4640 |