Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | >= 683 MPa | >= 99000 psi | |
Materion ToughMet® T3 CX105 (OD≥4") ToughMet® is Brush Wellman's solution for severe service material problems. By applying their EquaCast® process, tailored alloying additions and spinodal hardening technology, they have e.. |
|||
Tensile Strength, Ultimate | 683 MPa @Temperature 649 °C |
99100 psi @Temperature 1200 °F |
|
Haynes Ultimet® alloy, 6.3-38.1 mm plate Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Tensile Strength, Ultimate | 683 MPa @Temperature 23.0 °C |
99100 psi @Temperature 73.4 °F |
|
ATI Allegheny Ludlum Stainless Steel Free Machining Grade Type 416, Tempered at 704°C (UNS S41600) Allegheny Ludlum's 416 is a free-machining stainless steel specifically designed to exhibit improved machinability. These modifications retain, in so far as possible, the good mechanical properties.. |
|||
Tensile Strength, Ultimate | 683 MPa | 99100 psi | |
Haynes Hastelloy® G-30® alloy, 31.8 mm thick plate HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |