Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 674 MPa @Temperature 538 °C |
97800 psi @Temperature 1000 °F |
at 538°C after aging |
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 538°C (1000°F) Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man.. |