Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 662 MPa | 96000 psi | |
Hogen Duralloy H30W 80 Tungsten/20 Copper PM Metal Composite RWMA Class 12.Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 12 material is .. |
|||
Tensile Strength, Ultimate | 662 MPa | 96000 psi | |
Mi-Tech Metals CW80 80 Tungsten/20 Copper PM Metal Composite RWMA Class 12.Mi-Tech refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 12 material is specifi.. |
|||
Tensile Strength, Ultimate | 662 MPa @Temperature 204 °C |
96000 psi @Temperature 399 °F |
|
Haynes Hastelloy® C-22® alloy, 12.7-50.8 mm thick bar, solution heat treated HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Tensile Strength, Ultimate | 662 MPa | 96000 psi | |
Universal Wire Works 310 Cb Stainless Steel Electrode Universal 310 Cb electrodes are the same as the 310 electrodes except for the addition of columbium and the reduction in the carbon content. This alloy is especially useful in the welding of types 3.. |
|||
Tensile Strength, Ultimate | 662 - 752 MPa | 96000 - 109000 psi | |
Eagle Brass 511 Phosphor Bronzes 4%, Extra Spring 511 offers wear resistance, high strength, ductility, excellent spring properties and good bearing properties. Typical uses include fuse clips, switch parts, terminals, electronic connectors, bridge.. |
|||
Tensile Strength, Ultimate | >= 662 MPa | >= 96000 psi | |
Eagle Brass 752 Nickel Silver 18%, Extra Spring Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info.. |
|||
Tensile Strength, Ultimate | 662 MPa | 96000 psi | 1" thick plate as rolled |
EDRO #45 Free Machining Carbon Steel EDRO #45™ is a medium carbon steel stocked in as rolled condition. EDRO #45™ is characterized by: excellent machinability, responds to surface hardening, may be welded, and good dimensional stabil.. |
|||
Tensile Strength, Ultimate | 662 MPa @Temperature 538 °C |
96000 psi @Temperature 1000 °F |
H1150 |
Crucible Steel 15-5 Precipitation Hardening Stainless Steel Crucible 15-5 is a Premium Quality precipitation-hardening stainless steel which is capable of high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is a V.. |
|||
Tensile Strength, Ultimate | 662 MPa @Temperature 538 °C |
96000 psi @Temperature 1000 °F |
H1150 |
Crucible Steel 17Cr-4Ni Precipitation Hardening Stainless Steel Crucible 17Cr-4Ni is a precipitation-hardening stainless steel which is capable of a high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is martensitic a.. |
|||
Tensile Strength, Ultimate | 662 MPa @Temperature 538 °C |
96000 psi @Temperature 1000 °F |
H1150 |
Crucible Steel 17Cr-4Ni Super-X® Precipitation Hardening Stainless Steel Crucible 17Cr-4Ni is a version of 17CR-4Ni which has been modified to substantially improve machinability and other properties. Patented 17Cr-4Ni Super-X meets industry specifications for 17Cr-4Ni. .. |
|||
Tensile Strength, Ultimate | 662 MPa @Temperature 149 °C |
96000 psi @Temperature 300 °F |
|
Carpenter Gall-Tough® Stainless Data provided by Carpenter Technology Corporation.6.4 mm diameter tensile specimens from center of 25.4 mm diameter bar annealed 1066°C 1 hour, water quenched, and ground.Threshold Galling Stress 1.. |