Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 654 MPa @Temperature 260 °C |
94900 psi @Temperature 500 °F |
|
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, GTAW Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T.. |