Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 648 MPa | 94000 psi | |
Hogen Duralloy H20W 78 Tungsten/22 Copper PM Metal Composite RWMA Class 11 and 12.Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 12 mater.. |
|||
Tensile Strength, Ultimate | 648 MPa | 94000 psi | |
Mi-Tech Metals CW78 78 Tungsten/22 Copper PM Metal Composite RWMA Class 11 and 12.Mi-Tech refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 12 material is .. |
|||
Tensile Strength, Ultimate | 648 MPa @Temperature 260 °C |
94000 psi @Temperature 500 °F |
|
Haynes Hastelloy® C-22® alloy, all-weld metal, GMAW short arc HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Tensile Strength, Ultimate | 648 MPa | 94000 psi | Annealed Sheet, 0.15-1.6mm thick |
Special Metals INCOLOY® alloy 864 INCOLOY® alloy 8684 (UNS S35135) was specifically developed for automotive exhaust system flexible couplings, EGR tubes, manifolds and tailpipes. It exhibits excellent fatigue resistance, therma.. |
|||
Tensile Strength, Ultimate | 648 MPa | 94000 psi | |
Special Metals INCONEL® 690 Nickel Superalloy, Cold Drawn Tube, 3.50 inch (88.9 mm) o.d. and 0.219 inch (5.49 mm) Thickness Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Tensile strength (ultimate and yield) and elongation values reported here are typical for Cold Drawn Tube, 3.50 in.. |
|||
Tensile Strength, Ultimate | 648 - 710 MPa | 94000 - 103000 psi | |
Ametek High Purity Nickel Strip 899A Full Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Ultimate | 648 - 710 MPa | 94000 - 103000 psi | |
Ametek High Purity Nickel Strip 899L Full Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Ultimate | 648 - 710 MPa | 94000 - 103000 psi | |
Ametek High Purity Nickel Strip 899M Full Hard Information supplied by Ametek Specialty Metal Products.AMETEK High Purity Nickel offers major advantages to the rechargeable battery industry, including:Lowest electrical resistivity available in p.. |
|||
Tensile Strength, Ultimate | 648 MPa | 94000 psi | Annealed |
ATI Allegheny Ludlum 425 Mod Martensitic Stainless Steel Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for.. |
|||
Tensile Strength, Ultimate | 648 MPa | 94000 psi | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 10% Cold Rolled (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Tensile Strength, Ultimate | 648 MPa @Temperature 260 °C |
94000 psi @Temperature 500 °F |
|
Haynes Hastelloy® C-22® alloy, all-weld metal, GTAW HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |