Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 63.7 MPa | 9250 psi | DIN 53455; ASTM D638 |
Kolon SPESIN® KP212VO Flame Retardant PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Tensile Strength, Ultimate | 63.7 MPa | 9250 psi | ASTM D638 |
Kolon Kocetal® K300 General Purpose Grade Acetal Copolymer Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Tensile Strength, Ultimate | 63.7 MPa | 9250 psi | DIN 53455; ASTM D638 |
Kolon KOPA® KN333HI2 High Impact Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Tensile Strength, Ultimate | 63.7 MPa | 9250 psi | DIN 53455; ASTM D638 |
Kolon KOPA® KN133MT40 M/F Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Tensile Strength, Ultimate | 63.7 MPa | 9250 psi | |
Shinil Chemical SHINFLAME PC Flame Retardant Polymer Film SHINFLAME is a flame retardant (FR) compound which exhibits inherent flame retardant properties during fire. Shinil uses its patented dispersion blending technology with variety of polymers to prod.. |
|||
Tensile Strength, Ultimate | 63.7 MPa | 9240 psi | ASTM D1708 |
Daelim H&L Plavis-C DF Conductive Polyimide Bearing Direct Formed. Plavis-C: Conductive, Electrical conductive, high thermal resistance and superior mechanical properties. Surface resistivity 10²-10³ OhmGeneral Plavis information for all grades:PL.. |
|||
Tensile Strength, Ultimate | 63.7 MPa | 9240 psi | ASTM D1708 |
Daelim H&L Plavis-G15 DF 15% Graphite Filled Aromatic Polyimide Bearing Direct Formed. Plavis-G-15: Graphite 15 wt% filled, Self lubricating grade for wear and friction applications.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 ca.. |
|||
Tensile Strength, Ultimate | 63.7 MPa | 9240 psi | ASTM D1708 |
Daelim H&L Plavis-MS CM MoS2 Filled Aromatic Polyimide Bearing Compression Molded. Plavis-MS: MoS2 15 wt% filled, Self lubricating grade for vacuum environments.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 carbons is the .. |
|||
Tensile Strength, Ultimate | 63.7 MPa | 9240 psi | ASTM D1708 |
Daelim H&L Plavis-ESD DF Polyimide Bearing Direct Formed. Plavis-ESD: Electrostatic dissipative, Electrostatic dissipative, high thermal resistance and superior mechanical properties. And surface resistivity 10²-10³ OhmGeneral Plavis info.. |