Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 624 MPa
90500 psi
ASTM E8
ATI Allegheny Ludlum 310S Austenitic Stainless Steel
Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo..
Tensile Strength, Ultimate 624 MPa

@Temperature 593 °C
90500 psi

@Temperature 1100 °F
at 593°C after aging
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 593°C (1100°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac..