Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 621 MPa | 90000 psi | |
Pacific Sintered Materials FN-262-T High Strength Nickel Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability.Equivalent MPIF Specification: FN-0405-45All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Ultimate | 621 MPa | 90100 psi | |
Hogen Duralloy H10W 75 Tungsten/25 Copper PM Metal Composite RWMA Class 11.Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 11 Cu-W (a hard.. |
|||
Tensile Strength, Ultimate | 621 MPa | 90100 psi | |
Kennametal Stellite Stellite® 190 PM with P/M Processing Adhesive wear test data: P/M 0.32.Applications: vane plugs, fuel metering pins, spacer bushings, ball (bearings) blanks, race (bearings) blanks, diesel engine exhaust, fluid valve seats, saw cutter .. |
|||
Tensile Strength, Ultimate | 621 MPa @Temperature 760 °C |
90100 psi @Temperature 1400 °F |
|
Kennametal Stellite Stellite® 3 PM with P/M Processing Typical applications include (aerospace) vane plugs, fuel metering pins, spacer bushings, (bearings) ball blanks, race blanks, (valve seat inserts) diesel engine exhaust, fluid valve seats, saw cutt.. |
|||
Tensile Strength, Ultimate | 621 MPa | 90100 psi | ASTM D638 |
Glastic Laminates/Shapes HIR Grade HIR Fiberglass-Reinforced Polyester Rod Data provided by Glastic Corporation.A continuous-filament fiberglass-roving provides superior strength. Highest physical properties of GLASROD series. |
|||
Tensile Strength, Ultimate | 621 - 689 MPa | 90000 - 100000 psi | |
Materion BrushCAST® 3C High Conductivity Casting Alloy (Solution Annealed & Aged) Pouring Temperature: 1095-1175°CHeat treatment required for max strength (Annealing): 870-900°C/water quenchHeat treatment required for max strength (Hardening): 870-900°C/water quenchDescr.. |
|||
Tensile Strength, Ultimate | 621 MPa | 90000 psi | High Speed Steel (18 W, 4 Cr, 1 V) butt joint |
Lucas-Milhaupt EASY FLO Silver Based Cadmium-Bearing Filler Metal Applications: Easy-Flo is very versatile and can be used successfully on nearly all nickel, iron and copper base alloys. In certain instances, special fluxes, may be required to obtain good wettin.. |
|||
Tensile Strength, Ultimate | >= 621 MPa | >= 90100 psi | Annealed; AMS 4943 |
Haynes Ti-3Al-2.5V Alloy Titanium Tubing Haynes® Ti-3Al-2.5V alloy is both lightweight and strong, providing a major design advantage - saving weight.Specific alloying additives, notably aluminum, raise the temperature at which a titani.. |
|||
Tensile Strength, Ultimate | 621 - 827 MPa | 90000 - 120000 psi | |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed Strip Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Annealed Strip specifically. Other property values are typical of annealed DURANICKEL® alloy 3.. |
|||
Tensile Strength, Ultimate | 621 - 827 MPa | 90000 - 120000 psi | |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed Wire Tensile strength (ultimate) and elongation values reported here are typical for Annealed Wire specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the alloy in gen.. |
|||
Tensile Strength, Ultimate | 621 - 896 MPa | 90000 - 130000 psi | |
Special Metals DURANICKEL® 301 (UNS N03301) Hot-Finished Rod and Bar Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Hot-Finished Rod and Bar specifically. Other property values are typical of annealed DURANICKELÂ.. |
|||
Tensile Strength, Ultimate | >= 621 MPa | >= 90000 psi | Min per ASTM B582; Sheet and Plate |
Special Metals INCONEL® G-3 Nickel Superalloy Data provided by the manufacturer, Special Metals. |
|||
Tensile Strength, Ultimate | 621 MPa | 90000 psi | |
Universal Wire Works 90SB-3 Steel Welding Wire Universal 90SB-3 is a 2.25% chromium and 1% molybdenum alloy for welding on steel of similar composition. This alloy is designed for joints in process piping systems, boilers, or pressure vessels. W.. |
|||
Tensile Strength, Ultimate | 621 MPa | 90000 psi | |
Universal Wire Works E81T1-Ni2 Flux Cored Carbon Steel Tubular Electrode Alloys 81T1-Ni1 and Ni2 are designed for gas-shielded flux cored welding of low alloy steels that require good CVN toughness at subzero temperatures. These alloys are excellent for single and multip.. |
|||
Tensile Strength, Ultimate | 621 MPa | 90000 psi | AR-5% O2 |
Universal Wire Works ER90SB-9 Steel Welding Wire Universal 90S-B9 is used primarily for welding the higher chromium alloyed 9CrMoNbV steels A213 (T-91), A335 (p-91), A387 (Gr-91) used where elevated temperatures and pressures are required. The adv.. |
|||
Tensile Strength, Ultimate | 621 MPa | 90000 psi | |
Universal Wire Works 347 Stainless Steel (AMS 5680) Filler Metal Universal 347 is extensively used with the gas tungsten arc, gas metal arc and submerged arc processes. This alloy is suitable for welding stabilized steel grades 321, 347 and 348. Alloy 347 should .. |
|||
Tensile Strength, Ultimate | 621 - 758 MPa | 90000 - 110000 psi | |
Eagle Brass 7026 Copper Nickel, 1/2 Hard 7026 is a high performance alloy used in springs, terminals, elevated temperature interconnects and high reliability telecommunication components.Information provided by Eagle Brass Company |
|||
Tensile Strength, Ultimate | 621 - 724 MPa | 90000 - 105000 psi | |
Eagle Brass 7026 Copper Nickel, 1/4 Hard 7026 is a high performance alloy used in springs, terminals, elevated temperature interconnects and high reliability telecommunication components.Information provided by Eagle Brass Company |
|||
Tensile Strength, Ultimate | 621 - 724 MPa | 90000 - 105000 psi | |
Eagle Brass 70265 XP175, 1/4 Hard Information provided by Eagle Brass Company |
|||
Tensile Strength, Ultimate | 621 - 724 MPa | 90000 - 105000 psi | |
Eagle Brass 725 Copper Nickel Tin, Extra Spring Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Tensile Strength, Ultimate | 621 - 696 MPa | 90000 - 101000 psi | |
Eagle Brass 752 Nickel Silver 18%, Spring Alloy C752 combines corrosion resistance with strength and a lustrous silver color. Applications include optical frames and parts, springs, surgical instruments, jewelry, resistors and contacts.Info.. |
|||
Tensile Strength, Ultimate | 621 - 724 MPa | 90000 - 105000 psi | |
Eagle Brass 762 Nickel Silver 12%, Hard 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Tensile Strength, Ultimate | 621 MPa | 90000 psi | |
Crucible Steel 348 Chromium-Nickel Steel Crucible 348 is a non-hardenable austenitic chromium-nickel steel which are particularly adaptable for use at temperatures between 800 and 1650°F. This grade is non-magnetic in the annealed conditi.. |
|||
Tensile Strength, Ultimate | 621 MPa | 90100 psi | |
AK Steel 321 Austenitic Stainless steel AK Steel 321 is a stabilized austenitic stainless steel similar to Type 304 but with a titanium addition. This titanium addition reduces or prevents carbide precipitation during welding and in 427 .. |
|||
Tensile Strength, Ultimate | 621 MPa | 90100 psi | |
Carpenter Invar 36® Alloy, Cold Drawn Bars Data provided by Carpenter Technology Corporation.Carpenter Invar "36" alloy is a 36% nickel-iron alloy possessing a rate of thermal expansion approx. one-tenth that of carbon steel up to 200°C. T.. |
|||
Tensile Strength, Ultimate | 621 MPa | 90100 psi | ASTM E8 |
ATI Allegheny Ludlum 309 Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Tensile Strength, Ultimate | 621 MPa | 90100 psi | |
ATI Allvac® Nickelvac® 601 UNS N06601 Nickel Superalloy Uses: Weld wire, woven wire mesh belts, rod for heat treat baskets, heat treat fixtures.Property values are for samples in the metallurgical condition: 1950°C anneal.Information provided by Allvac,.. |
|||
Tensile Strength, Ultimate | 621 MPa | 90000 psi | |
PSM Industries Pacific Sintered Metals High Carbon Copper Steel FCC-214-S(HT) Powdered Metal High strength, Good impact resistant material for mechanical components, Excellent hardenability, High performance material with high strength and wear resistance after heat treatment Equivalent MP.. |