Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 62.05 MPa | 9000 psi | |
Abatron AboCast 8-2/Abocure 8-2 Epoxy
(discontinued **) 2-part solvent-free dielectric epoxy casting compound.Processing: 100/50 ratio (pbw); Gel time, 100 g (3.5 oz.): 265 minutes; cures in 3 weeks at 25°C (77°F).Applications: solventless casting, adh.. |
|||
Tensile Strength, Ultimate | 62.05 MPa | 9000 psi | |
Abatron AboCast 8-13/Abocure 8-13 Epoxy
(discontinued **) 2-part, clear, solvent-free dielectric epoxy casting compound.Processing: 100/12.80 ratio (pbw); Gel time, 100 g (3.5 oz.): 53 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°.. |
|||
Tensile Strength, Ultimate | 62.05 MPa | 9000 psi | |
Abatron AboCast/AboCure 8109-2 High melting point. Filled version.Processing: 100/10 pbw; 90 minute potlife; mix at 130-140°C (270 °F); cures in 16 h/120°C (250°F), 10 h/140°C (285°F), 8 h/160°C (320°F), 2 h/ 200°C (390°.. |
|||
Tensile Strength, Ultimate | 62.05 MPa | 9000 psi | |
Abatron AboCast/AboCure 8109-4 Safety hardener (minimum toxicity) version of 8109-3.Processing: 100/10 pbw; Potlife: 2.5 h/20°C (68°F), 30 min/40°C (105°F), 15 min/60°C (140°F); mix at RT; cures in: 24 h/20°C (68°F), 2-3 .. |
|||
Tensile Strength, Ultimate | 62.05 MPa | 9000 psi | |
Abatron AboCast/AboCure 8109-9 Minimum toxicity version of 8109-8.Processing: 100/25 ratio; Potlife: 45 min/20°C (68°F), 20 min/40°C (105°F), 10 min /60°C (140°F); mix at RT; cures in: 24 h/20°C (68°F), 2-3 h/60°C (140°.. |