Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 6.0688 MPa

@Temperature 260 °C
880.21 psi

@Temperature 500 °F
Air Aging, 70 hours; ASTM D1414
Freudenberg Simrit S310 Silicone Elastomer (VMQ)
General Purpose; AMS 3301; A-A-59588 (ZZ-R-765) Class 2A, 2B Grade 40; Good heat resistance. Poor resistance to abrasion, tear and cut growth; low tensile strength; inferior resistance to oil, gasol..