Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 57.9 MPa | 8400 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Stat-Tech™ PF-NX-062100-2 Polysulfone
(discontinued **) Description/Features:Electrically ConductiveESD ProtectionInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Ultimate | 57.9 - 57.9 MPa @Temperature 150 - 150 °C |
8400 - 8400 psi @Temperature 302 - 302 °F |
Average value: 57.9 MPa Grade Count:1 |
Overview of materials for Thermoplastic Polyimide, Unfilled |
|||
Tensile Strength, Ultimate | 57.9 MPa @Temperature 150 °C |
8400 psi @Temperature 302 °F |
ASTM D638 |
Mitsui AURUM® 450 Thermoplastic Polyimide Resin, Non-filled
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Tensile Strength, Ultimate | 57.9 MPa | 8400 psi | ASTM D638 |
Plenco 2424 Phenolic, Granular, Injection Molded
(discontinued **) Two-stage Phenolic. PLENCO 02424 is a black, two stage, general purpose phenolic molding compound. It has a good balance of properties for a general purpose type material. It is used in electrical .. |
|||
Tensile Strength, Ultimate | 57.9 MPa | 8390 psi | ASTM D412 |
SK Chemicals SKYTHANE® 155D S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Ultimate | 57.9 MPa | 8390 psi | ASTM D412 |
SK Chemicals SKYTHANE® S155D Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tensile Strength, Ultimate | 57.9 MPa | 8400 psi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 8600-10 Polycarbonate EMERGEâ„¢ PC 8600-10 is a translucent, ignition-resistant polycarbonate resin. The resin contains no bromine, chlorine or phosphate additives and is intended to comply with global environmental .. |
|||
Tensile Strength, Ultimate | 57.9 MPa | 8400 psi | ASTM D412; ASTM D638 |
Lubrizol Estane® 58610 Thermoplastic Polyurethane Features: Combines flexibility, toughness and excellent roll release for calendering and melt coating applications.Uses: Injection molding and general extrusion techniques. It is used in film, shee.. |
|||
Tensile Strength, Ultimate | 57.9 MPa | 8400 psi | |
AdvanSource Biomaterials ChronoFlex® AL 55D Biodurable Medical Grade Polyurethane ChronoFlex® AL is a family of premium polycarbonate aliphatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® AL medical-grade el.. |